← All topics · Core

Materials Science

Crystal structures, mechanical properties, phase diagrams, corrosion. ~4–7%

About 4 min read · 11 sections

Overview

Materials questions are mostly definitions, comparisons and a few short calculations. This guide groups the ideas the way the exam does: structure, mechanical behaviour, phase diagrams, heat treatment, corrosion and the main material families.

1. Atomic structure and crystals

StructureAtoms per cellCoordinationPacking factor
Simple cubic160.52
BCC280.68
FCC4120.74
HCP6120.74

Iron is BCC at room temperature (ferrite) and FCC at high temperature (austenite). FCC metals such as copper and aluminum are generally more ductile. Defects (vacancies, dislocations, grain boundaries) control strength: more obstacles to dislocation motion means a stronger but less ductile metal.

2. Mechanical properties

A tensile test gives the stress–strain curve.

  • Modulus of elasticity E: slope of the linear region (stiffness).
  • Yield strength: stress at the onset of permanent deformation; use the 0.2% offset method if there is no clear yield point.
  • Ultimate tensile strength: the peak of the engineering curve.
  • Ductility: percent elongation or percent reduction in area.
  • Toughness: energy absorbed to fracture, the area under the stress–strain curve; resilience is the area up to yield.

Hardness tests (Brinell, Rockwell, Vickers) measure resistance to indentation and correlate with tensile strength. The Charpy impact test measures toughness and reveals the ductile-to-brittle transition of steels at low temperature.

True stress σ_T = σ(1 + ε); engineering strain ε = ΔL/L₀

Stress concentrations at holes and notches raise the local stress: σ_max = K_t σ_nominal.

3. Fatigue, creep and fracture

  • Fatigue: failure under repeated loading at stresses below yield. Steels have an endurance limit below which life is effectively infinite; aluminum does not.
  • Creep: slow, time-dependent strain under constant load, serious at temperatures above about 0.4 of the melting temperature.
  • Brittle fracture occurs with little plastic deformation, driven by flaws; fracture toughness K_Ic measures resistance.

4. Phase diagrams

A phase diagram shows which phases are stable at each temperature and composition. For a tie line across a two-phase region, the lever rule gives phase fractions.

W_α = (C_β − C₀)/(C_β − C_α), W_β = (C₀ − C_α)/(C_β − C_α)

Lever rule

Given: an alloy of 30 wt% B lies in a two-phase region where the α phase is 10 wt% B and the β phase is 60 wt% B.

Solution: W_β = (30 − 10)/(60 − 10) = 0.40 and W_α = 0.60.

The iron–carbon diagram has a eutectoid at 0.77 wt% C and 727 °C, where austenite transforms into pearlite (alternating ferrite and cementite). Steel has up to about 2.1 wt% C; cast iron has more. Hypoeutectoid steels (below 0.77% C) contain proeutectoid ferrite plus pearlite.

5. Heat treatment of steel

TreatmentResult
Annealingslow cool; soft, ductile, stress-free
Normalizingair cool; finer grains, moderate strength
Quenchingfast cool; hard, brittle martensite
Temperingreheat after quenching; trades hardness for toughness

Hardenability is how deeply a steel can be hardened; alloying elements increase it. Cold working increases strength and reduces ductility (strain hardening); annealing restores ductility by recrystallization.

6. Corrosion

Corrosion is an electrochemical process. Oxidation occurs at the anode (metal loss) and reduction at the cathode. In a galvanic cell the more active metal in the galvanic series becomes the anode and corrodes faster. Protection methods: coatings, galvanizing (a sacrificial zinc anode), cathodic protection, inhibitors, and choosing compatible metals. Other types include pitting, crevice, stress-corrosion cracking and intergranular attack.

7. Polymers, ceramics and composites

  • Thermoplastics soften when heated and can be reshaped. Thermosets are cross-linked and decompose rather than melt. Elastomers are lightly cross-linked and very stretchy.
  • Ceramics are hard, strong in compression, brittle and resist heat and corrosion.
  • Composites combine materials. For fibres aligned with the load, the upper-bound modulus follows the rule of mixtures:
E_c = V_f E_f + V_m E_m

Rule of mixtures

Given: 60% fibre by volume (E = 200 GPa) in a matrix with E = 3 GPa.

Solution: E_c = 0.6(200) + 0.4(3) = 121.2 GPa along the fibres.

Common mistakes

  • Confusing strength (stress to fail) with stiffness (modulus).
  • Mixing up toughness (area under the whole curve) with hardness (resistance to indentation).
  • Treating the iron–carbon eutectoid composition as 4.3% (that is the eutectic).
  • Forgetting that the more active metal is the one that corrodes in a galvanic couple.

Exam strategy

Many questions can be answered by definition alone. Learn the vocabulary, memorize the three numbers (0.77% C, 727 °C, 4.3% C), and use the lever rule only after identifying the tie-line endpoints correctly.

Checklist

  • [ ] I know the atoms per cell, coordination and packing factors for FCC, BCC and HCP.
  • [ ] I can read a stress–strain curve and define yield, UTS, ductility and toughness.
  • [ ] I can apply the lever rule and describe the iron–carbon eutectoid.
  • [ ] I can match heat treatments to their results.
  • [ ] I can explain galvanic corrosion and common protection methods.