Overview
Construction materials questions focus on concrete and its ingredients, aggregates, asphalt, steel and timber. They test definitions, standard tests and a few short calculations (strength from a cylinder, water–cement ratio, absorption, fineness modulus, mix proportions).
1. Concrete basics
Concrete = cement + water + aggregates (+ admixtures). Hydration of cement and water produces strength over time; the 28-day compressive strength f′_c is the reference.
- Water–cement ratio w/c = weight of water ÷ weight of cement. Lower w/c means higher strength and lower permeability (Abrams' law); adding water on site hurts strength and durability.
- Workability is measured by the slump test; higher slump means a wetter, more fluid mix.
- Air entrainment (4–7%) improves freeze–thaw durability but slightly lowers strength.
- Curing keeps concrete moist and warm so hydration continues.
Cylinder strength
Given: a 6 in diameter cylinder fails at 90,000 lb.
Solution: A = π(6)²/4 = 28.27 in². f′_c = 90,000/28.27 = 3,183 psi.
Normal-weight concrete weighs about 150 lb/ft³; 10 yd³ (270 ft³) is about 40,500 lb. Elastic modulus E_c = 57,000√f′_c psi.
2. Mix design (absolute volume method)
Each ingredient occupies a volume = weight ÷ (specific gravity × 62.4 lb/ft³). The volumes of cement, water, air and aggregates add up to 27 ft³ per cubic yard.
Absolute-volume mix
Given: per yd³: cement 564 lb (SG 3.15), water 282 lb, air 6%, aggregates SG 2.65 with sand 40% of the aggregate volume.
Solution: cement 564/(3.15 × 62.4) = 2.87 ft³; water 282/62.4 = 4.52 ft³; air 0.06 × 27 = 1.62 ft³. Aggregate volume = 27 − 2.87 − 4.52 − 1.62 = 17.99 ft³. Sand = 0.4(17.99) = 7.20 ft³ → 7.20(2.65)(62.4) = 1,190 lb. Gravel = 10.79 ft³ → 1,785 lb.
3. Aggregates
- Gradation: sieve analysis gives percent passing = 100 − cumulative percent retained.
- Fineness modulus FM = Σ(cumulative % retained on the standard sieves)/100; fine sand about 2.3–3.1.
- Absorption = (SSD mass − oven-dry mass)/oven-dry mass × 100. The saturated-surface-dry (SSD) state is the reference condition for mix design.
Fineness modulus
Given: cumulative percent retained on #4, #8, #16, #30, #50, #100: 3, 15, 35, 60, 85, 97.
Solution: sum = 295, so FM = 2.95.
Moisture correction: stockpile aggregate carries free moisture. Wet weight = SSD weight × (1 + MC)/(1 + Abs); subtract the free water from the mixing water.
Moisture correction
Given: a batch needs 1,190 lb of SSD sand. Stockpile moisture content = 5%, absorption = 1%.
Solution: wet sand = 1,190(1.05)/(1.01) = 1,237 lb. Free water = 1,237 − 1,190 = 47 lb, so reduce the mixing water by 47 lb.
4. Asphalt
Asphalt concrete is aggregate bound with asphalt binder. Binder is graded by performance grade PG X−Y: X is the 7-day maximum pavement temperature (°C) and Y is the minimum (°C), so PG 64−22 resists rutting to 64 °C and cracking to −22 °C. Mix design (Marshall or Superpave) targets about 4% air voids and adequate voids in mineral aggregate. Too much binder causes bleeding and rutting; too little causes raveling and cracking.
5. Steel
Mild steel has a distinct yield plateau; high-strength steels use the 0.2% offset yield. Modulus is about 29,000 ksi (200 GPa) for all steels. Common grades: A36 (F_y = 36 ksi) and A992 (F_y = 50 ksi). Rebar is graded by yield strength (Grade 60 means 60 ksi), and bar number = diameter in eighths of an inch. Strain in the elastic range: ε = σ/E; 36 ksi gives ε = 0.00124.
Thermal expansion: ΔL = αLΔT. For concrete α ≈ 5.5×10⁻⁶ per °F, so a 100 ft slab warming by 60 °F grows 0.40 in; steel and concrete have similar α, which makes reinforced concrete work.
6. Timber and masonry
Timber strength depends on species, grade, moisture content and load duration. Moisture content = (wet weight − dry weight)/dry weight. A sample weighing 12 lb wet and 10 lb dry has MC = 20%. Wood shrinks as it dries and is strongest parallel to the grain. Masonry (brick, concrete block) is strong in compression and requires reinforcing and mortar of suitable type.
7. Standard tests at a glance
| Test | Measures |
|---|---|
| Slump | workability of fresh concrete |
| Compression cylinder | f′_c at 7, 28 days |
| Sieve analysis | aggregate gradation |
| Proctor | maximum dry density of soil |
| Marshall | asphalt stability and flow |
| Charpy | impact toughness |
Common mistakes
- Using the weight of water-to-total instead of water-to-cement in w/c.
- Forgetting the 62.4 lb/ft³ factor when converting weight to volume.
- Calling the passing percentage the retained percentage.
- Forgetting that free moisture in aggregate adds water to the mix.
- Mixing PG temperature units (they are °C).
Exam strategy
Group each question by material, recall the one standard test or formula that applies, and write the units. When a choice suggests adding water to improve workability, it is almost always wrong.
Checklist
- [ ] I can compute w/c, cylinder strength and the modulus of concrete.
- [ ] I can compute fineness modulus, absorption and moisture corrections.
- [ ] I can proportion a mix by the absolute volume method.
- [ ] I can interpret an asphalt PG grade.
- [ ] I know the common steel grades and rebar sizes.